DIN EN 1.4571 Material, X6CrNiMoTi17-12-2 Stainless Steel
Embed This Widget
Add the script tag and a data attribute to embed this widget.
Embed via iframe for maximum compatibility.
<iframe src="https://alloyfyi.com/iframe/entity/din-en-14571-material-x6crnimoti17-12-2-stainless-steel/" width="420" height="400" frameborder="0" style="border:0;border-radius:10px;max-width:100%" loading="lazy"></iframe>
Paste this URL in WordPress, Medium, or any oEmbed-compatible platform.
https://alloyfyi.com/entity/din-en-14571-material-x6crnimoti17-12-2-stainless-steel/
Add a dynamic SVG badge to your README or docs.
[](https://alloyfyi.com/entity/din-en-14571-material-x6crnimoti17-12-2-stainless-steel/)
Use the native HTML custom element.
Add one script tag to your page:
<div data-alloyfyi="entity" data-slug="din-en-14571-material-x6crnimoti17-12-2-stainless-steel"></div>
<script src="https://cdn.jsdelivr.net/npm/alloyfyi-embed@1/dist/embed.min.js" defer></script>
Embed as an iframe:
<iframe src="https://alloyfyi.com/iframe/entity/din-en-14571-material-x6crnimoti17-12-2-stainless-steel/?style=modern&theme=light" width="420" height="400" frameborder="0" loading="lazy" style="border:0;border-radius:10px;max-width:100%"></iframe>
Paste the URL in WordPress, Medium, or Ghost:
https://alloyfyi.com/ar/alloys/din-en-14571-material-x6crnimoti17-12-2-stainless-steel/
Shields.io-compatible SVG badge:

Web Component:
<alloyfyi-entity slug="din-en-14571-material-x6crnimoti17-12-2-stainless-steel"></alloyfyi-entity>
<script src="https://cdn.jsdelivr.net/npm/alloyfyi-embed@1/dist/embed.min.js" defer></script>
العائلة: Stainless Steel
تقييمات الأداء
Performance Radar
| خاصية | Rating |
|---|---|
| Strength | 6 / 10 |
| Corrosion Res. | 7 / 10 |
| Lightweight | 5 / 10 |
| Machinability | 3 / 10 |
| Affordability | 6 / 10 |
| Heat Res. | 7 / 10 |
التركيب
الخصائص الميكانيكية
| مقاومة الشد | 500.0 MPa |
| حد الخضوع | 235.0 MPa |
| الاستطالة | 40.0% |
| الصلابة (برينل) | 215.0 HB |
| الصلابة (روكويل) |
التركيب الكيميائي
| العنصر | النسبة المئوية (%) |
|---|---|
| Cr | 16.5-18.5 |
| Mo | 2.00-2.50 |
| Ni | 10.5-13.0 |
| Ti | 5xC-0.70 |
| C ≤ | 0.08 |
| P ≤ | 0.045 |
| S ≤ | 0.015 |
| Mn ≤ | 2.00 |
| Si ≤ | 1.00 |
| Country (Regions) | European Union |
| ISO Name (ISO Number) | X6CrNiMoTi17-12-2 (4571-316-35-I) |
| Steel Name (Material Number) | X6CrNiMoTi17-12-2 (1.4571) |
أين تشتري DIN EN 1.4571 Material, X6CrNiMoTi17-12-2 Stainless Steel
قد تكسب الروابط عمولة دون أي تكلفة إضافية عليك.
الوصف
DIN EN 1.4571 material (X6CrNiMoTi17-12-2) is made by adding titanium (Ti) to EN 1.4401 stainless steel (X5CrNiMo17-12-2) to improve the resistance to intergranular corrosion. Titanium can improve the corrosion resistance of stainless steel, especially intergranular corrosion, effectively prevent the sensitization of stainless steel, and also improve the stability of steel in high temperature and high pressure. When the mass fraction of titanium is between 0.03% and 0.1%, the yield strength of the steel is improved. Therefore, EN 1.4571 material has higher temperature resistance, corrosion resistance and sensitization resistance than 1.4401. EN 1.4571 is more resistant to corrosion than EN 1.4301 (X5CrNi18-10) and 1.4401 (X5CrNiMo17-12-2). Because it contains titanium and forms TiC with carbon, it greatly reduces the risk of intergranular corrosion sensitization. However, in high temperature, high concentration of concentrated nitric acid, chloride and hot alkaline solution, significant corrosion may occur. EN 1.4571 steel has good weldability, does not require preheating before welding, and usually does not require heat treatment after welding.