DIN EN 1.4571 Material, X6CrNiMoTi17-12-2 Stainless Steel vs SAE AISI 4130 Chromoly Steel, Alloy Material Properties, Chemical Composition

Ratings Comparison

Strength

DIN EN 1.4571 Material, X6CrNiMoTi17-12-2 Stainless Steel 6/10
SAE AISI 4130 Chromoly Steel, Alloy Material Properties, Chemical Composition 6/10

Corrosion Resistance

DIN EN 1.4571 Material, X6CrNiMoTi17-12-2 Stainless Steel 7/10
SAE AISI 4130 Chromoly Steel, Alloy Material Properties, Chemical Composition 3/10

Lightweight

DIN EN 1.4571 Material, X6CrNiMoTi17-12-2 Stainless Steel 5/10
SAE AISI 4130 Chromoly Steel, Alloy Material Properties, Chemical Composition 5/10

Machinability

DIN EN 1.4571 Material, X6CrNiMoTi17-12-2 Stainless Steel 3/10
SAE AISI 4130 Chromoly Steel, Alloy Material Properties, Chemical Composition 6/10

Cost Efficiency

DIN EN 1.4571 Material, X6CrNiMoTi17-12-2 Stainless Steel 6/10
SAE AISI 4130 Chromoly Steel, Alloy Material Properties, Chemical Composition 9/10

Temperature Resistance

DIN EN 1.4571 Material, X6CrNiMoTi17-12-2 Stainless Steel 7/10
SAE AISI 4130 Chromoly Steel, Alloy Material Properties, Chemical Composition 7/10

Properties Comparison

Property DIN EN 1.4571 Material, X6CrNiMoTi17-12-2 Stainless Steel SAE AISI 4130 Chromoly Steel, Alloy Material Properties, Chemical Composition
Metal Base Stainless Steel Steel
Tensile Strength 500.0 MPa 670.0 MPa
Yield Strength 235.0 MPa 435.0 MPa
Elongation 40.0 % 25.5 %
Hardness (Brinell) 215.0 HB 197.0 HB
Elastic Modulus
Density
Melting Point
Thermal Conductivity
Weldable
Heat Treatable
Magnetic