304 Stainless Steel Properties: SS304 Composition, Density, Yield Strength, Thermal Conductivity, Hardness, Modulus of Elasticity vs AISI 301 Stainless Steel Properties, Type 301 Full Hard SS Grade Spring (UNS S30100)

Ratings Comparison

Strength

304 Stainless Steel Properties: SS304 Composition, Density, Yield Strength, Thermal Conductivity, Hardness, Modulus of Elasticity 6/10
AISI 301 Stainless Steel Properties, Type 301 Full Hard SS Grade Spring (UNS S30100) 5/10

Corrosion Resistance

304 Stainless Steel Properties: SS304 Composition, Density, Yield Strength, Thermal Conductivity, Hardness, Modulus of Elasticity 7/10
AISI 301 Stainless Steel Properties, Type 301 Full Hard SS Grade Spring (UNS S30100) 7/10

Lightweight

304 Stainless Steel Properties: SS304 Composition, Density, Yield Strength, Thermal Conductivity, Hardness, Modulus of Elasticity 5/10
AISI 301 Stainless Steel Properties, Type 301 Full Hard SS Grade Spring (UNS S30100) 5/10

Machinability

304 Stainless Steel Properties: SS304 Composition, Density, Yield Strength, Thermal Conductivity, Hardness, Modulus of Elasticity 4/10
AISI 301 Stainless Steel Properties, Type 301 Full Hard SS Grade Spring (UNS S30100) 4/10

Cost Efficiency

304 Stainless Steel Properties: SS304 Composition, Density, Yield Strength, Thermal Conductivity, Hardness, Modulus of Elasticity 6/10
AISI 301 Stainless Steel Properties, Type 301 Full Hard SS Grade Spring (UNS S30100) 6/10

Temperature Resistance

304 Stainless Steel Properties: SS304 Composition, Density, Yield Strength, Thermal Conductivity, Hardness, Modulus of Elasticity 7/10
AISI 301 Stainless Steel Properties, Type 301 Full Hard SS Grade Spring (UNS S30100) 7/10

Properties Comparison

Property 304 Stainless Steel Properties: SS304 Composition, Density, Yield Strength, Thermal Conductivity, Hardness, Modulus of Elasticity AISI 301 Stainless Steel Properties, Type 301 Full Hard SS Grade Spring (UNS S30100)
Metal Base Stainless Steel Stainless Steel
Tensile Strength 585.0 MPa
Yield Strength 235.0 MPa
Elongation 60.0 %
Hardness (Brinell) 149.0 HB
Elastic Modulus
Density
Melting Point
Thermal Conductivity
Weldable
Heat Treatable
Magnetic

Related Comparisons