Alle Legierungen

Durchsuchen Sie unsere umfassende Legierungsdatenbank.

Alle Steel Stainless Steel Aluminum Copper Titanium Nickel Zinc Magnesium Tin Lead Cobalt Tungsten Precious Metal Other

MPEA Al1 Li0.062 Mg0.062 Sn0.062 Zn0.062

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Zugfestigkeit: 836,0 MPa Streckgrenze: 415,0 MPa

MPEA Al1 Nb1 Ta1 Ti1 V1

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: BCC. Processing: CAST.

Streckgrenze: 993,0 MPa

MPEA Co0.476 Cr0.476 Fe0.476 Nb0.095 Ni1

Nickel

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Zugfestigkeit: 698,5 MPa Streckgrenze: 365,0 MPa

MPEA Co0.5 Fe0.5 Mo0.5 Ni1 V0.5

Nickel

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

MPEA Co0.625 Fe0.625 Mo0.625 Ni1 V0.625

Nickel

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

MPEA Co0.875 Cr0.625 Fe1 Ni1

Steel

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: FCC. Processing: WROUGHT.

Zugfestigkeit: 721,0 MPa Streckgrenze: 241,0 MPa

MPEA Co1 Cr0.429 Fe0.571 Mo0.286 Ni0.571

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: FCC. Processing: CAST.

Zugfestigkeit: 1194,0 MPa Streckgrenze: 879,0 MPa

MPEA Co1 Cr0.667 Fe0.667 Ni1 Ti0.667

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: ANNEAL.

MPEA Co1 Cr1 Cu1 Fe1 Ni1 Ti0.5

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: FCC. Processing: CAST.

Zugfestigkeit: 1650,0 MPa Streckgrenze: 700,0 MPa

MPEA Co1 Cr1 Cu1 Fe1 Ni1 V0.042

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Streckgrenze: 303,0 MPa

MPEA Co1 Cr1 Fe1 Mn1 Mo0.042 Ni1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: FCC. Processing: CAST.

Streckgrenze: 225,0 MPa

MPEA Co1 Cr1 Fe1 Mn1 Mo0.19 Ni1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Streckgrenze: 765,0 MPa

MPEA Co1 Cr1 Fe1 Mn1 Ni1 Ta0.6

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: .

MPEA Co1 Cr1 Fe1 Mn1 Ni1 V0.75

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: ANNEAL.

Zugfestigkeit: 1325,0 MPa Streckgrenze: 740,0 MPa

MPEA Co1 Cr1 Fe1 Mo0.208 Ni1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Zugfestigkeit: 589,6 MPa Streckgrenze: 254,7 MPa

MPEA Co1 Cr1 Fe1 Nb0.155 Ni1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Zugfestigkeit: 744,0 MPa Streckgrenze: 322,0 MPa

MPEA Co1 Cu1 Fe1 Mn1 Ni1 Sn0.03

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: FCC. Processing: CAST.

Zugfestigkeit: 465,0 MPa

MPEA Co1 Cu1 Fe1 Mn1 Ni1 Sn0.2

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Zugfestigkeit: 368,0 MPa

MPEA Cr1 Cu1 Fe1 Mo1 Ni1

Other

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: FCC. Processing: CAST.

MPEA Cr1 Fe1 Ni1 Ti0.2

Other

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Streckgrenze: 2297,9 MPa

MPEA Al1 Co1 Cu1 Fe1 Ni1 Ti1

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Streckgrenze: 1612,0 MPa

MPEA Al1 Co1 Cu1 Fe1 Ni0.5

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Streckgrenze: 929,0 MPa

MPEA Al1 Cr1 Fe1 Mo0.5 Ni1 Ti0.4

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Zugfestigkeit: 3673,4 MPa Streckgrenze: 2185,1 MPa

MPEA Al1 Cr1 Fe1 Mo0.8 Ni1

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Zugfestigkeit: 1513,0 MPa Streckgrenze: 1513,0 MPa

MPEA Al1 Cr1 Nb1 Ti1 V1

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: ANNEAL.

Zugfestigkeit: 977,5 MPa Streckgrenze: 937,5 MPa

MPEA Al1 Nb1 Ta1 Ti1

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: BCC. Processing: CAST.

Streckgrenze: 740,0 MPa

MPEA Al1 Nb1 Ti1 V1 Zr0.25

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: ANNEAL.

Zugfestigkeit: 1260,0 MPa Streckgrenze: 1065,0 MPa

MPEA Co1 Cr1 Fe1 Ni1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: FCC. Processing: WROUGHT.

Zugfestigkeit: 708,0 MPa Streckgrenze: 360,0 MPa

MPEA C0.429 Co1 Cr1 Fe1 Ni1 W0.429

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: FCC. Processing: POWDER.

MPEA Co0.086 Cu0.086 Fe0.086 Nb1 Ni0.086

Other

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: WROUGHT.

Streckgrenze: 1703,0 MPa

MPEA Co0.5 Fe0.5 Mo0.1 Ni1 V0.25

Nickel

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: FCC. Processing: CAST.

Streckgrenze: 233,0 MPa

MPEA B0.035 Co0.207 Cr0.207 Fe1 Mn0.621

Steel

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

MPEA Co0.986 Cr0.952 Fe0.933 Mn0.914 Ni1

Nickel

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: BCC. Processing: WROUGHT.

Zugfestigkeit: 995,0 MPa Streckgrenze: 852,5 MPa

MPEA Co1 Cr0.667 Fe0.667 Ni1 Ti0.333

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: ANNEAL.

MPEA Co1 Cr1 Cu1 Fe1 Ni1 Ti1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: FCC. Processing: CAST.

Zugfestigkeit: 1272,0 MPa Streckgrenze: 1272,0 MPa

MPEA Co1 Cr1 Fe1 Mn1 Ni1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: FCC. Processing: CAST.

Zugfestigkeit: 688,0 MPa Streckgrenze: 494,8 MPa

MPEA Co1 Cr1 Fe1 Mn1 Ni1 V0.5

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: FCC. Processing: CAST.

Streckgrenze: 620,0 MPa

MPEA Co1 Cr1 Fe1 Mo0.304 Ni1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Zugfestigkeit: 1054,3 MPa Streckgrenze: 665,2 MPa

MPEA Co1 Cr1 Fe1 Nb0.103 Ni1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Zugfestigkeit: 622,0 MPa Streckgrenze: 318,0 MPa

MPEA Co1 Cr1 Fe1 Ni1 Ti0.3

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: FCC. Processing: WROUGHT.

Zugfestigkeit: 772,0 MPa Streckgrenze: 540,0 MPa

MPEA Co1 Cu1 Fe1 Mn1 Ni1 Sn0.05

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Zugfestigkeit: 475,0 MPa

MPEA Co1 Cu1 Fe1 Ni1 Ti1 V1 Zr1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

MPEA Co1 Fe1 Mo0.8 Ni1 V1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

MPEA Co0.273 Cr0.477 Nb0.477 Ni0.045 Ti1

Titanium

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

MPEA Co1 Cr1 Cu1 Ni1 Zn1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: POWDER.

Streckgrenze: 2121,0 MPa

MPEA Al1 Cr1 Fe1 Mo0.2 Ni1

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Zugfestigkeit: 3222,0 MPa Streckgrenze: 1487,0 MPa

MPEA Co1 Cr1 Cu1 Fe1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: FCC. Processing: .

MPEA Co1 Cr1 Cu0.5 Fe1 Ni1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: FCC. Processing: CAST.