AA 7020 Aluminum Alloy vs AA 7034 Aluminum Alloy

Ringkasan

AA 7020 Aluminum Alloy and AA 7034 Aluminum Alloy are both aluminum alloys commonly used in engineering applications. 7020 Aluminum offers a tensile strength of 401 MPa compared to 7034 Aluminum's 647 MPa.

Key Differences

Perbandingan Peringkat

Kekuatan

AA 7020 Aluminum Alloy 5/10
AA 7034 Aluminum Alloy 6/10

Ketahanan korosi

AA 7020 Aluminum Alloy 6/10
AA 7034 Aluminum Alloy 6/10

Ringan

AA 7020 Aluminum Alloy 9/10
AA 7034 Aluminum Alloy 9/10

Kemampuan mesin

AA 7020 Aluminum Alloy 8/10
AA 7034 Aluminum Alloy 8/10

Efisiensi Biaya

AA 7020 Aluminum Alloy 7/10
AA 7034 Aluminum Alloy 7/10

Ketahanan Suhu

AA 7020 Aluminum Alloy 4/10
AA 7034 Aluminum Alloy 4/10

Perbandingan Sifat

Property AA 7020 Aluminum Alloy AA 7034 Aluminum Alloy
Logam dasar Aluminum Aluminum
Kekuatan tarik 401.0 MPa 647.0 MPa
Kekuatan luluh 305.5 MPa 593.0 MPa
Perpanjangan 13.8 % 1.9 %
Kekerasan (Brinell)
Modulus Elastis
Kepadatan
Titik Leleh
Konduktivitas termal
Dapat Dilas
Dapat Diperlakukan Panas
Magnetik

Kapan Menggunakan AA 7020 Aluminum Alloy

Choose 7020 Aluminum when your application specifically requires this aluminum alloy's unique combination of properties and industry certifications.

Kapan Menggunakan AA 7034 Aluminum Alloy

Choose 7034 Aluminum when you need superior strength.

Frequently Asked Questions

Which is stronger, 7020 or 7034?
7020 has a tensile strength of 401 MPa while 7034 reaches 647 MPa, making 7034 the stronger alloy in ultimate tensile terms. For yield strength, 7020 is rated at 305.5 MPa versus 593 MPa for 7034.
Does 7020 or 7034 have better corrosion resistance?
Both alloys share the same corrosion resistance rating of 6/10.
Is 7020 or 7034 easier to weld?
Weldability data is not available for both alloys. In terms of machinability, 7020 scores 8/10 and 7034 scores 8/10.
Which is more cost-effective, 7020 or 7034?
Both alloys are similarly priced with a cost rating of 7/10.
Can I use 7020 instead of 7034 for aerospace applications?
Strength ratings: 7020 5/10 vs 7034 6/10. Always validate substitution against your specific design codes and operating conditions.