Stress Corrosion Cracking
Embed This Widget
Add the script tag and a data attribute to embed this widget.
Embed via iframe for maximum compatibility.
<iframe src="https://alloyfyi.com/iframe/glossary/stress-corrosion-cracking/" width="420" height="400" frameborder="0" style="border:0;border-radius:10px;max-width:100%" loading="lazy"></iframe>
Paste this URL in WordPress, Medium, or any oEmbed-compatible platform.
https://alloyfyi.com/glossary/stress-corrosion-cracking/
Add a dynamic SVG badge to your README or docs.
[](https://alloyfyi.com/glossary/stress-corrosion-cracking/)
Use the native HTML custom element.
Add one script tag to your page:
<div data-alloyfyi="glossary" data-slug="stress-corrosion-cracking"></div>
<script src="https://cdn.jsdelivr.net/npm/alloyfyi-embed@1/dist/embed.min.js" defer></script>
Embed as an iframe:
<iframe src="https://alloyfyi.com/iframe/glossary/stress-corrosion-cracking/?style=modern&theme=light" width="420" height="400" frameborder="0" loading="lazy" style="border:0;border-radius:10px;max-width:100%"></iframe>
Paste the URL in WordPress, Medium, or Ghost:
https://alloyfyi.com/id/glossary/stress-corrosion-cracking/
Web Component:
<alloyfyi-glossary slug="stress-corrosion-cracking"></alloyfyi-glossary>
<script src="https://cdn.jsdelivr.net/npm/alloyfyi-embed@1/dist/embed.min.js" defer></script>
Corrosion & Protection
Definition
A failure mechanism involving the simultaneous action of a corrosive environment and sustained tensile stress, leading to crack initiation and propagation at stress levels below the material's yield strength.
Detailed Explanation
Stress corrosion cracking (SCC) is highly material- and environment-specific: austenitic stainless steels are susceptible to SCC in chloride environments, while brass is attacked by ammonia (season cracking). The cracks typically propagate intergranularly or transgranularly and can be catastrophic because they grow without significant plastic deformation or visible warning. Prevention strategies include reducing tensile stress (shot peening, stress relief), selecting resistant alloys, or eliminating the corrosive species.