MPEA Al0.7 Co0.3 Cr1 Fe1 Ni1

Other

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: POWDER.

Zugfestigkeit: 2635,0 MPa Streckgrenze: 2033,0 MPa

MPEA Al1 Co0.149 Cr0.34 Cu0.191 Fe0.34 Ni0.106

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: .

MPEA Al1 Co0.238 Cr0.714 Cu0.119 Fe0.167 Ni0.143

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: .

MPEA Al1 Co0.256 Cr0.795 Cu0.128 Fe0.205 Ni0.179

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: .

MPEA Al1 Co0.304 Cr0.5 Cu0.109 Fe0.152 Ni0.109

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: .

MPEA Al1 Co0.333 Cr0.333 Fe0.333 Ni0.333

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: BCC. Processing: CAST.

MPEA Al1 Co0.419 Cr0.558 Fe0.233 Ni0.116

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: .

MPEA Al1 Co0.512 Cr0.512 Fe0.186 Ni0.116

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: .

MPEA Al0.278 Co0.694 Cr0.222 Fe0.417 Ni1 Ti0.167

Nickel

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Zugfestigkeit: 660,0 MPa Streckgrenze: 486,5 MPa

MPEA Al1 Co0.5 Cr1 Fe0.147 Ni0.294

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: .

MPEA Al1 Co0.833 Cr0.833 Fe0.833 Ni0.833 Ti0.667

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Streckgrenze: 1503,0 MPa

MPEA Al1 Co1 Cr1 Cu1 Fe1 Ni1 V1

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Streckgrenze: 1469,0 MPa

MPEA Al1 Co1 Cr1 Fe1 Ni1 Si0.4

Aluminum

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: BCC. Processing: CAST.

Zugfestigkeit: 2444,0 MPa Streckgrenze: 1481,0 MPa

MPEA Al0.417 Co0.833 Cr0.833 Cu0.833 Fe0.833 Ni0.833 Ti1

Titanium

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

MPEA Al0.569 Ca0.143 Li0.857 Mg1 Si0.286 Y0.003

Other

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Streckgrenze: 556,0 MPa

MPEA Al0.544 C0.001 Co0.69 Fe1 Ni0.69

Steel

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Streckgrenze: 1202,0 MPa

China 8Cr13MoV Stainless Steel, Blade Steel Review, Hardness, Datasheet, Specification

Stainless Steel

Stainless Steel

AA 7068 Aluminum Alloy

Aluminum

Aluminum Alloy

Zinc Alloy (Al-Zn). AA designation 7068.

Zugfestigkeit: 623,0 MPa

MPEA Al0.511 Co0.511 Cr0.511 Fe0.511 Ni1

Nickel

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: .

Zugfestigkeit: 1030,0 MPa Streckgrenze: 562,5 MPa

MPEA Al0.4 Hf0.6 Nb1 Ta1 Ti1 Zr1

Other

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: BCC. Processing: OTHER.

Zugfestigkeit: 834,0 MPa Streckgrenze: 547,0 MPa

MPEA Al0.581 Co0.968 Cr0.323 Fe0.323 Mo0.032 Ni1

Nickel

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Streckgrenze: 1159,7 MPa

MPEA Al0.5 Co0.5 Cr0.5 Fe1 Mo0.25 Ni0.5

Steel

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

MPEA Al0.5 Co1 Cr0.5 Fe0.5 Mo0.25 Ni0.5

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

MPEA Al0.5 Co1 Cr1 Cu1 Fe1 Ni1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Zugfestigkeit: 790,0 MPa Streckgrenze: 399,5 MPa

MPEA Al0.5 Co1 Cr1 Cu1 Fe1 Ni1 Ti0.2

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: FCC. Processing: CAST.

MPEA Al0.5 Co1 Cr1 Cu1 Fe1 Ni1 Ti1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

MPEA Al0.5 Co1 Cr1 Cu1 Fe1 Ni1 V0.4

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

MPEA Al0.5 Co1 Cr1 Cu1 Fe1 Ni1 V0.6

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

MPEA Al0.5 Co1 Cr1 Cu1 Fe1 Ni1 V1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

MPEA Al0.5 Co1 Cr1 Fe1 Mn1 Ni1 Ta0.2

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: .

ASTM A572 Grade 50 Steel Equivalent, Gr 65, 60 Properties, Tensile Yield Strength

Steel

MPEA Al0.5 Co1 Cr1 Fe1 Ni1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: ANNEAL.

MPEA Al0.5 Co1 Fe1 Ni1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Streckgrenze: 346,0 MPa

MPEA Al0.5 Cr1 Cu1 Fe1 Ni1

Other

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: FCC. Processing: CAST.

MPEA Al0.5 Hf1 Nb1 Ta1 Ti1 Zr1

Other

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: BCC. Processing: CAST.

Streckgrenze: 1302,0 MPa

MPEA Al0.5 Mo1 Nb1 Ti1 V1

Other

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: BCC. Processing: CAST.

Zugfestigkeit: 1800,0 MPa Streckgrenze: 1625,0 MPa

MPEA Al0.5 Nb1 Ta1 Ti1 V1

Other

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: BCC. Processing: CAST.

Streckgrenze: 1014,0 MPa

MPEA Al0.667 C1 Co0.667 Cr0.667 Fe0.667 Ni0.667

Other

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Zugfestigkeit: 2083,0 MPa Streckgrenze: 1255,0 MPa

MPEA Al0.667 Co0.667 Cu0.667 Fe0.667 Ni1

Nickel

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Streckgrenze: 680,0 MPa

MPEA Al0.667 Co1 Cr0.667 Fe0.667 Mo0.333 Ni0.667

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

MPEA Al0.667 Cr1 Nb0.667 Ti0.667 V0.667

Other

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: ANNEAL.

Zugfestigkeit: 1262,5 MPa Streckgrenze: 1170,0 MPa

MPEA Al0.667 Li0.667 Mg0.333 Sc0.667 Ti1

Titanium

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: .

MPEA Al0.667 Nb1 Ta0.333 Ti1 Zr0.333

Other

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: BCC. Processing: OTHER.

Zugfestigkeit: 1000,0 MPa Streckgrenze: 728,0 MPa

MPEA Al0.6 Co1 Cr0.333 Fe0.333 Mo0.067 Ni1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Streckgrenze: 1250,8 MPa

MPEA Al0.43 Co1 Cr1 Fe1 Mn1 Ni1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

Streckgrenze: 285,0 MPa

MPEA Al0.714 Cr0.714 Cu0.714 Fe0.714 Ni1

Nickel

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: ANNEAL.

MPEA Al0.75 Co1 Cr1 Fe1 Mn1 Ni1

Cobalt

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: other. Processing: CAST.

MPEA Al0.417 Co0.833 Cr0.833 Cu0.833 Fe0.833 Ni0.833 V1

Other

High-Entropy Alloy (MPEA)

High-entropy alloy. Phase: BCC. Processing: CAST.