Resumo
AA 2009 Aluminum Alloy and AA 2017 Aluminum Alloy are both aluminum alloys commonly used in engineering applications. 2009 Aluminum offers a tensile strength of 457.5 MPa compared to 2017 Aluminum's 425 MPa.
Key Differences
- ◆ {'alloy_a': '457.5 MPa', 'alloy_b': '425 MPa', 'property': 'Tensile Strength'}
- ◆ {'alloy_a': '332 MPa', 'alloy_b': '275 MPa', 'property': 'Yield Strength'}
- ◆ {'alloy_a': 'N/A', 'alloy_b': 'N/A', 'property': 'Hardness (Brinell)'}
- ◆ {'alloy_a': 'N/A', 'alloy_b': 'N/A', 'property': 'Density'}
- ◆ {'alloy_a': 'N/A', 'alloy_b': 'N/A', 'property': 'Melting Point'}
- ◆ {'alloy_a': '5/10', 'alloy_b': '5/10', 'property': 'Strength Rating'}
- ◆ {'alloy_a': '6/10', 'alloy_b': '6/10', 'property': 'Corrosion Rating'}
- ◆ {'alloy_a': '7/10', 'alloy_b': '7/10', 'property': 'Cost Rating'}
- ◆ {'alloy_a': '8/10', 'alloy_b': '8/10', 'property': 'Machinability Rating'}
- ◆ {'alloy_a': '4/10', 'alloy_b': '4/10', 'property': 'Temperature Rating'}
- ◆ {'alloy_a': '9/10', 'alloy_b': '9/10', 'property': 'Weight Rating'}
Comparação de classificações
Resistência
AA 2009 Aluminum Alloy
5/10
AA 2017 Aluminum Alloy
5/10
Resistência à corrosão
AA 2009 Aluminum Alloy
6/10
AA 2017 Aluminum Alloy
6/10
Leve
AA 2009 Aluminum Alloy
9/10
AA 2017 Aluminum Alloy
9/10
Maquinabilidade
AA 2009 Aluminum Alloy
8/10
AA 2017 Aluminum Alloy
8/10
Eficiência de custos
AA 2009 Aluminum Alloy
7/10
AA 2017 Aluminum Alloy
7/10
Resistência à temperatura
AA 2009 Aluminum Alloy
4/10
AA 2017 Aluminum Alloy
4/10
Comparação de propriedades
| Property | AA 2009 Aluminum Alloy | AA 2017 Aluminum Alloy |
|---|---|---|
| Metal base | Aluminum | Aluminum |
| Resistência à tração | 457.5 MPa | 425.0 MPa |
| Limite de elasticidade | 332.0 MPa | 275.0 MPa |
| Alongamento | 86.0 % | 23.8 % |
| Dureza (Brinell) | — | — |
| Módulo elástico | — | — |
| Densidade | — | — |
| Ponto de fusão | — | — |
| Condutividade térmica | — | — |
| Soldável | — | — |
| Tratável termicamente | — | — |
| Magnético | — | — |
Quando usar AA 2009 Aluminum Alloy
Choose 2009 Aluminum when your application specifically requires this aluminum alloy's unique combination of properties and industry certifications.
Quando usar AA 2017 Aluminum Alloy
Choose 2017 Aluminum when your application specifically requires this aluminum alloy's unique combination of properties and industry certifications.
Frequently Asked Questions
Which is stronger, 2009 or 2017?
2009 has a tensile strength of 457.5 MPa while 2017 reaches 425 MPa, making 2009 the stronger alloy in ultimate tensile terms. For yield strength, 2009 is rated at 332 MPa versus 275 MPa for 2017.
Does 2009 or 2017 have better corrosion resistance?
Both alloys share the same corrosion resistance rating of 6/10.
Is 2009 or 2017 easier to weld?
Weldability data is not available for both alloys. In terms of machinability, 2009 scores 8/10 and 2017 scores 8/10.
Which is more cost-effective, 2009 or 2017?
Both alloys are similarly priced with a cost rating of 7/10.